The test material is put on a chair simulation and is exposed to a burning cigarette.
A test rig is constructed, and exposed to a burning cigarette covered with sheeting material. The cigarette has to burn its entire length.
The test material is categorised Class I or Class II. If an obvious ignition occurs, the material is Class II. If not, the char on the vertical panel is measured to determine the classification.